Monday, 10 November 2008

Ready to De-Mould, well almost




















I filled the mould

To get the most real looking and accurate surface I did two things.
-Stippling in paraffin wax onto areas of the mould surface adds small random areas of damage.
-A loose powdering of the mould meant that the top surface should be a shiny aluminium appearance.

mixing a ration of 100g resin(coloured white) to 75g aluminium powder to 75g iron powder,
In totally the mould required around 450g of resin. If my plans are correct, the dusted aluminium will give a shiny top surface, and where the wax will be removed will reveal the lower darker surface...Hopefully making the key appear very authentic.

De mould tomorrow morning, was going to do it today, but temperature was very cold and resin was catalysing very slowly. So didn't want to rush and risk it deforming....