De moulded the fibre glass and removed the former for the key, there were 2 little problems but they were easily over come. Before pouring the second half of the silicone I re polished one side of the key. In doing this I must have rubbed away the releasing agent in some area's and the two parts fused together. But they were scalpled apart and the mould was un damaged.
--There was one section where the silicone did not catalyse compeltely, there must have been something on the key to in hibit it, but never found out what.

Cleaned out the mould with some fast cast, and the surface is very good. On monday I will cast with polyester resin and metal powders.
Battery Update
Also turned all the componets for the battery, details will be lazer cut on monday, hopefully lacqured by the end of the day.....